Mormate

Description: Casting slip additive to increase dry strength

Notes

MORMATE Ceramic Processing Additive is a specialty chemical additive formulated to increase the green strength (Modulus of Rupture) of a water based slip/slurry system. Due to this unique formulation, it also increases the permeability of the system. Desired processing benefits are easily achieved by using the additive at proper levels.

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Additives for Ceramic Glazes
Materials that are added to glazes to impart physical working properties and usually burn away during firing. In industry all glazes, inks and engobes have additives, they are considered essential to control of cohesion, adhesion, suspension, dry hardness, surface leveling, rheology, speed-of-drying, etc. Among potters, it is common for glazes to have zero additives.