Arcilla de Pontezuelo (Cuba)

Description: Cuban clay

Oxide Analysis Formula Tolerance
SiO2 64.80% 4.69
Al2O3 23.45% 1.00
Fe2O3 0.42% 0.01
TiO2 0.65% 0.04
CaO 0.39% 0.03
MgO 0.63% 0.07
K2O 2.07% 0.10
Na2O 0.37% 0.03
LOI 6.44%n/a
Oxide Weight 403.56
Formula Weight 431.34

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
Materials Caolín Gris (Cuba)
Materials Caolín Blanco (Cuba)
Materials Caolín Mantua (Cuba)
Materials Caolín Damanueco (Cuba)
Materials Caolín Santa Elena (Cuba)
Materials Arcilla Revolucion I (Cuba)
Materials Arcilla Revolucion II (Cuba)
Materials Arcilla Revolucion III (Cuba)
Materials Arcilla Club de Cazadores (Cuba)
Materials Barro Ovas (Cuba)
Materials Ciego de Avila (Cuba)

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy