Alternate Names: Ferro Frit 5325
Description: Low melting high expansion sodium borosilicate fluorine frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 2.36% | 0.14 | |
| K2O | 2.59% | 0.09 | |
| Na2O | 14.77% | 0.77 | |
| F | 2.72% | 0.47 | |
| Al2O3 | 7.97% | 0.25 | |
| B2O3 | 13.81% | 0.64 | |
| SiO2 | 55.77% | 3.01 | |
| Oxide Weight | 324.87 | ||
| Formula Weight | 324.87 | ||
Was known as Ferro Frit 5325
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Fusion Frit 5325
|
| Materials |
Ferro Frit 5325P
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk