Matrix Frit B40-C

Description: High boron zero silicate refractory calcia alumina frit

Oxide Analysis Formula Tolerance
B2O3 40.00% 1.34
Al2O3 33.00% 0.76
CaO 24.00% 1.00
Oxide Weight 226.74
Formula Weight 226.74

Notes

Although this frit is very high in boron, it is a refractory (this might be a surprise to ceramic technicians who are accustomed to the use of boron as a powerful flux). Frits of this type have been in use to stop the penetration of aluminum in refractories since 1958 (by Carborundum Co., Metaullics Inc., Ceradyne, H-W Refractories (now ANH), and AP Green, and others). The original patent holder for these frits was Kaiser Aluminum Corp.

They are about ~1% soluble after 90 min in ~25 C water. In this way they can be used in castable cements where any appreciable amount of soluble boric oxide would retard Calcium Aluminate cement almost indefinitely.

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Matrix Frit B70-A
Materials Calcium Aluminate Cement
Oxides B2O3 - Boric Oxide