| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 1.96% | 0.07 | |
| Na2O | 6.47% | 0.34 | |
| CaO | 4.06% | 0.24 | |
| BaO | 2.46% | 0.05 | |
| ZnO | 1.37% | 0.05 | |
| Li2O | 2.26% | 0.25 | |
| Al2O3 | 3.81% | 0.12 | |
| B2O3 | 26.13% | 1.23 | |
| SiO2 | 51.49% | 2.80 | |
| Oxide Weight | 326.56 | ||
| Formula Weight | 326.56 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.3 x 10-6 |
|---|---|
| Frit Melting Range (C) | 1300F |