Alternate Names: Fusion Frit 578
Description: High barium zero boron frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 3.80% | 0.12 | |
| Na2O | 1.40% | 0.07 | |
| CaO | 5.60% | 0.30 | |
| BaO | 25.50% | 0.51 | |
| Al2O3 | 13.00% | 0.39 | |
| SiO2 | 50.70% | 2.56 | |
| Oxide Weight | 303.88 | ||
| Formula Weight | 303.88 | ||
| URLs |
http://www.fusionceramics.com/
Fusion Ceramics Frit Website |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.2 x 10-6 |
|---|---|
| Frit Softening Point | 1800F |
| By Tony Hansen Follow me on ![]() | ![]() |