Fusion Frit FZ-583

Alternate Names: Frit FZ583

Description: Barium Zinc Zero Boron frit

Oxide Analysis Formula Tolerance
BaO 37.00% 0.50
ZnO 16.00% 0.41
SiO2 40.00% 1.39
Al2O3 4.00% 0.08
Na2O 1.50% 0.05
K2O 1.50% 0.03
Oxide Weight 209.19
Formula Weight 209.19

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
By Tony Hansen
Follow me on

Got a Question?