Gers Borate 9/97

Description: Plastic Calcium Borate, Borocalcite

Oxide Analysis Formula Tolerance
CaO 19.12% 0.64
Na2O 4.30% 0.13
Al2O3 1.63% 0.03
B2O3 27.76% 0.75
SiO2 11.77% 0.37
MgO 4.20% 0.20
K2O 1.38% 0.03
Fe2O3 0.48% 0.01
LOI 29.35%n/a
Oxide Weight 133.52
Formula Weight 188.99

Notes

Since this material varied so much over the years, Ron Roy has been using various dated versions of the analysis, this is one of them.

Related Information

Links

Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy