Quartz 761

Alternate Names: Kuvars 761

Oxide Analysis Formula Tolerance
CaO 0.08% 0.06
K2O 0.16% 0.07
Na2O 0.27% 0.18
Al2O3 2.41% 1.00
SiO2 96.90% 68.24
LOI 0.18%n/a
Oxide Weight 4,224.75
Formula Weight 4,232.37

Notes

Available in -100, -63 and -45 micron sizes.