Alternate Names: Kuvars 762
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.14% | 0.27 | |
| SiO2 | 98.60% | 175.13 | |
| Al2O3 | 0.63% | 0.66 | |
| TiO2 | 0.04% | 0.05 | |
| Fe2O3 | 0.04% | 0.03 | |
| MgO | 0.15% | 0.40 | |
| Na2O | 0.09% | 0.15 | |
| K2O | 0.16% | 0.18 | |
| LOI | 0.15% | n/a | |
| Oxide Weight | 10,658.90 | ||
| Formula Weight | 10,674.92 | ||
Available in -100, -63 and -45 micron sizes.