Description: Andalusite/Pyrophyllite Ore
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 0.20% | 0.01 | |
| Na2O | 0.20% | 0.02 | |
| Al2O3 | 20.00% | 1.00 | |
| SiO2 | 75.00% | 6.36 | |
| Fe2O3 | 0.60% | 0.02 | |
| LOI | 2.80% | n/a | |
| Oxide Weight | 489.60 | ||
| Formula Weight | 503.70 | ||
Similar size and bulk density to 2253, but with slightly higher iron content.
| Materials |
Pyrotrol
|
| URLs |
https://www.rescoproducts.com/docs/default-source/data-sheets-us/sds/pyrotrol-all-grades-msds.pdf?sfvrsn=905bb13b_5
SDS for all versions of Pyrotrol |
| URLs |
https://www.rescoproducts.com/docs/default-source/data-sheets-us/pds/pyrotrol-2253-and-2254-and-3503.pdf
Pyrotrol Data Sheet |
| Bulk Density lbs/cu. ft. (Packed) | 45 |
|---|---|
| Pyrometric Cone Equivalent | 26 |
| Sieve Analysis Dry | +200 mesh: 1% |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk