Pyrofrac 4205

Oxide Analysis Formula Tolerance
K2O 0.20% 0.02
Na2O 0.20% 0.03
TiO2 0.40% 0.04
Al2O3 12.00% 1.00
SiO2 82.80% 11.71
Fe2O3 1.00% 0.05
SO4 3.00%n/a
H2O 3.40%n/a
Oxide Weight 821.10
Formula Weight 877.24

Notes

Used in structural clay coatings, refractory formulations, whiteware ceramics, art pottery to
increase refractoriness, reduce shrinkage, and widen firing range.
This material is made by crushing & screening of selectively mined andalusite/pyrophyllite/sericite ores
with heavy media separation.

Related Information

Links

Materials Andalusite
Materials Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc.
Materials Alkatrol
Materials Pyrofrac
Materials Seriphyl

Data

Bulk Density lbs/cu. ft. (Packed) 105
Pyrometric Cone Equivalent 23
Sieve Analysis Dry +20 mesh: 5.0 +50 mesh: 90.0 +70 mesh: 5.0
Density (Specific Gravity) 2.6