Arroyo Slip

Description: Albany Slip Substitute

Oxide Analysis Formula Tolerance
SiO2 64.00% 5.55
Al2O3 14.30% 0.73
Fe2O3 8.50% 0.28
TiO2 0.90% 0.06
MgO 3.50% 0.45
CaO 3.80% 0.35
K2O 3.50% 0.19
Oxide Weight 513.72
Formula Weight 513.72

Notes

It is a low-melting iron stained clay (hits zero porosity around cone 1). Very plastic (11% drying shrinkage) and slow drying (Albany Slip, by contrast, is non plastic and fast drying). Alberta Slip is more plastic than Albany, but not nearly as plastic as this.

Related Information

Arroyo Slip powder


This picture has its own page with more detail, click here to see it.

Melt fluidity of Albany Slip vs. Arroyo Slip at cone 10R


This picture has its own page with more detail, click here to see it.

Arroyo Slip fired test bars show its fired maturity at low temperatures


This picture has its own page with more detail, click here to see it.

Fired at cone 01, 02, 03, 06 (top to bottom).

Links

URLs http://www.lagunaclay.com/msds/Arroyo%20Slip.pdf
MSDS
Materials Albany Slip
A pure low plasticity clay that, by itself, melted to a glossy dark brown glaze at cone 10R. It was a popular glaze ingredient for many decades.
Materials Alberta Slip
Albany Slip successor - a plastic clay that melts to dark brown glossy at cone 10R, with a frit addition it can also host a wide range of glazes at cone 6.
Materials Jasper Slip
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy