ABC Colemanite

Description: California colemanite

Oxide Analysis Formula Tolerance
Fe2O3 0.10% -
SiO2 0.60% 0.02
B2O3 42.60% 1.12
Al2O3 0.20% -
SrO 1.00% 0.02
Na2O 0.10% -
MgO 0.30% 0.01
CaO 29.60% 0.97
LOI 25.50%n/a
Oxide Weight 136.36
Formula Weight 183.04

Related Information

Links

Materials Ulexite
A natural source of boron, it melts at a very low temperature to a clear glass.
Materials Colemanite
A natural source of boron that melts at a very low temperature.
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy