Sylvite

Alternate Names: Potassium chloride, KCL, Silvin, Silvine

Description: Soluble source of K2O

Oxide Analysis Formula Tolerance
K2O 52.44% 1.00
Cl 47.56%n/a
Oxide Weight 94.20
Formula Weight 179.63

Notes

This can be used as an alternative to NaCl in the salt glaze process.

Related Information

Links

Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Oxides K2O - Potassium Oxide
Minerals Sylvite
Soluble source of K2O.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy