Ceramitalc 10A

Oxide Analysis Formula Tolerance
CaO 6.94% 0.15
MgO 29.00% 0.85
Na2O 0.18% -
Al2O3 0.28% -
SiO2 56.80% 1.12
Fe2O3 0.20% -
MnO 0.13% -
LOI 6.46%n/a
Oxide Weight 110.53
Formula Weight 118.16

Notes

No longer available.

Related Information

Links

Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Materials Ceramitalc
Hazards Talc Hazards Overview
Talc is invaluable in the ceramics industry, it is used as a glaze and body ingredient and as a parting a release agent in various processes. Is it safe?
By Tony Hansen