BPS High Alkaline Frit

Description: Frit

Oxide Analysis Formula Tolerance
BaO 7.04% 0.09
CaO 2.86% 0.10
K2O 10.09% 0.21
Li2O 0.15% 0.01
Na2O 18.66% 0.59
B2O3 3.55% 0.10
Al2O3 5.20% 0.10
SiO2 52.44% 1.71
Oxide Weight 196.00
Formula Weight 196.00

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.