Onmillion Feldspar

Description: LOW IRON FELDSPAR

Oxide Analysis Formula Tolerance
K2O 10.00% 0.72
Na2O 2.50% 0.28
Al2O3 18.00% 1.20
SiO2 66.80% 7.59
Fe2O3 0.10% -
Oxide Weight 664.94
Formula Weight 664.94

Notes

A high grade material suitable for deflection yoke for TV, glass, frits, porcelain, tiles.

K2O is >= 10.0, Na2O >= 2.5, Fe2O3 <= 0.1

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy