3DP | BSG | AIF | ABR | | BIN | ADV | AGT | PHY | ASR | ALM | uAz | ALS | E11 | JWK | ART | ARC | EBA | LAG | PBA | BLC | NFi | mQi | BIN | 62N | BIO | BSQ | CHP | BDT | BGD | BGP | BFR | Csu | DZc | BRK | HWi | SCS | MCB | SCB | ECS | CSP | OLC | CRE | CPM | CRS | STN | CST | LBS | TIL | C3D | CBM | CLM | ECM | CLO | SLR | CRT | CCT | CLT | GBG | CCO | CCN | CRP | d3S | CGS | OCS | DEC | DFT | TM2 | | Dux | DRP | DSP | ELE | ELT | SEU | MUE | EEE | MEQ | SCE | EQD | EQP | EQM | EMR | SER | EQS | | ETC | P3D | PAR | PAU | PCA | PBF | PDE | PGL | PKB | PMM | PPO | PPP | PSH | PWT | EXT | FEL | TAA | FRC | 9h6 | FLB | kK5 | FLS | FRT | MFM | YtL | F3D | EGK | GNM | DGE | GBC | GBS | GLS | GLI | GLC | GLM | GLR | GLT | MGL | FGE | GLZ | GEQ | EHE | HMT | h79 | HTR | CHS | Niv | I3D | ICS | IDP | IGR | EAP | ISO | Qno | KAO | qhK | KCD | EKB | KIL | MKL | SKL | LNS | LAB | vLv | FRL | 7hb | LEM | CQL | LTR | MSH | MOF | MAN | | MRK | MDS | MMC | MPC | MTS | MTT | | MAM | MAA | MDE | MTE | EMP | MPE | CLM | DEN | PWH | MAT | e38 | MTR | BDW | PMF | MIN | 3MM | MMK | EMM | MNC | EMF | yPu | NOX | SOC | | DSL | OPA | QKk | OXI | RED | PTT | SWS | PPS | PNC | PRP | | SPM | MPB | SPB | FRP | 9Hv | POI | PEN | PTW | PEQ | a87 | EPR | PRS | PRT | | PRD | PRO | | | | QCC | RMP | RSR | MRM | SRM | MGR | RFR | wWm | REF | EAR | SRS | ESK | SWR | | SCU | | YFh | SIL | ESR | LrD | YnJ | ESP | MSM | Tmx | STC | OLS | k67 | JXh | PWS | TWC | EPW | TCP | TCE | WSN | TLS | MTL | STL | TGR | OTR | | | UNI | UVR | FWK | gLF | WRS | WPS | YQd

Gerstley Borate Substitutes

Many development efforts to create Gerstley Borate substitutes took place during the early 2000s (the initial period when the demise of Gerstley Borate appeared imminent). A number of companies, including Laguna Clays itself, produced and sold these for many years. When Laguna secured another stockpile at the mine and began producing the original material again, interest in substitutes gradually waned. However, the sudden dramatic price increase in 2023 appears to have initiated the process again. Gillespie Borate appears to be the only viable and visible substitute now.

Thus, the substitutes listed here are mostly no longer made. Other high-boron materials shown are also no longer available.

We continue to recommend sourcing B2O3 from frits instead. Please contact us if you have a specific recipe and we can work with you in your Insight-live account to develop a new recipe that both eliminates the GB and improves overall working and firing properties.

Related Information

Gerstley Borate substitutes chemistry comparison - ca. 2005


This picture has its own page with more detail, click here to see it.

Links

Materials Ulexite
A natural source of boron, it melts at a very low temperature to a clear glass.
Materials Colemanite
A natural source of boron that melts at a very low temperature.
Materials PotteryCrafts Frit P2954
A calcium borate frit (with extremely high boron).
Materials Ferro Frit 4112
A calcium borate frit (with extremely high boron).
Materials Turkish Colemanite
A mineral with very high B2O3 and CaO content.
Materials Turkish Ulexite
A mineral with very high B2O3 and CaO content.
Materials Ferro Frit 3134
A frit with 23% B2O3. The most common of frits used in pottery in North America. Around the world, other companies make frits of equivalent chemistry.
Materials Gerstley Borate
Gerstley Borate was a natural source of boron for ceramic glazes. It was plastic and melted clear at 1750F. Now we need to replace it. How?
Materials IMCO Borate
A Gerstley Borate substitute that was available during the early 2000s.
Materials Murrays Borate
A Gerstley Borate substitute that was available during the early 2000s.
Materials Laguna Borate
A Gerstley Borate substitute that was available during the early 2000s.
Materials Fusion Frit F-309
Materials Gillespie Borate
A Gerstley Borate substitute that became available during the early 2000s and is still available in 2023.
Materials Boraq
This Gerstley Borate substitute was available during the early 2000s. Its recipe and development are well documented but two materials are no longer available.
Typecodes Common Gerstley Borate glaze recipes
Many of the glazes in use are built on common base recipes. And there are some universal recipes that almost everyone uses, we may have already converted those for use with frits.
Typecodes Gerstley Borate Glaze Calculation examples
Examples of how we use glaze calculations (in an Insight-Live.com account) to replace Gerstley Borate with other materials, especially frits, in various glaze recipes. In doing so we take the opportunity to improve the recipe in other ways (e.g. reduce thermal expansion, improve slurry properties, reduce bubbling and crawling).
Media Use Insight-live to substitute materials in a recipe
We will substitute wollastonite for whiting and a frit for Gerstley borate in the G2571A cone 10 matte while maintaining the chemistry of the original recipe.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy