44MR | APPO | AVPS | AVSC | BDGC | BDLB | BLOI | BWIW | CCON | CDRY | CEC | CLWC | CMST | COLE | COVB | CSSS | DENS | DFAC | DFDM | DIEL | DNLP | DS | DSHR | DSRN | DSTR | DTMP | EBCT | EM20 | FRFU | FRRD | FRTG | FSHR | FSTR | GBBT | GBMF | GEBR | GLAZ | GLFL | GLHD | GLLE | GSPT | GTTM | HDMI | HEGF | HMA | HMAN | HMOH | IFP | IWCT | L10M | L1M | L20M | L2M | L30M | L5 | L5M | LDW | LOI | LQLM | MDPS | MLRG | MOIP | MOR | MOR5 | MORD | OLAD | P200 | P325 | PBPO | PCE | pHPG | pHPW | PPD | PRSM | PSHP | RC | RHEO | SADR | SAMG | SCLE | SHAB | SIEV | SLBY | SOLU | SPHC | SSAB | SVWT | TGA | THCO | TNST | TREL | TRMN | TSFL | UPSD | WABS | WOPL | WRA | WSR | XREF

WABS - Water absorption Test

An indicator of the density and therefore degree of vitrification of a fired clay body. Typically a body sample is fired at a range of temperatures and absorption measurements are done on each to produce a graph of porosity vs. temperature. Absorption is measured by weighing a bar before and after boiling in water and calculating the percentage increase in weight. Use the SHAB test to compile this information.

Variables

VAL - Value (V)

Enter the percent porosity and temperature

Related Information

Links

Tests Shrinkage/Absorption Test
SHAB Shrinkage and absorption test procedure for plastic clay bodies and materials
Typecodes Body Tests
Tests conducted on bodies made from materials, as opposed to the materials themselves.
URLs http://www.astm.org/Standards/C373.htm
ASTM-C373 Water Absorption

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy