03DSFF - Cone 03 Fast Fire
04DSDH - Low Temperature Drop-and-Hold
BQ1000 - Plainsman Electric Bisque Firing Schedule
BRTF05 - Bartlett Fast Glaze Cone 05
BRTF6 - Bartlett Fast Glaze Cone 6
BRTS6 - Bartlett Slow Glaze Cone 6
BTFB04 - Bartlett Fast Bisque Cone 04
BTSB04 - Bartlett Slow Bisque Cone 04
BTSG05 - Bartlett Slow Glaze Cone 05
C04PLTP - Plainsman Low Temperature Drop-and-hold
C10RPL - Plainsman Cone 10R Firing
C5DHSC - Plainsman Cone 5 Drop-and-Hold Slow-Cool
C6DHSC - Plainsman Cone 6 Drop-and-hold, Slow Cool
C6IRED - Cone 6 Iron Reds
C6MSGL1 - Mastering Glazes Cone 6
C6PLST - Plainsman Cone 6 Electric Standard
FSCG1 - Shimbo Crystal Schedule 1
FSCGB1 - Shimbo Crystal Holding Pattern 2
FSCGCL - Shimbo Crystal Celestite Schedule
FSCGWM - Wollast-O-Matte Fara Shimbo Crystalline Glaze
FSCRGL - GC106 Base for Crystalline Glazes
FSHP1 - Shimbo Crystal Holding Pattern 1
FSHP3 - Shimbo Crystal Holding Pattern 3
FSNM5 - Fa's Number Five
MDDCL - Medalta Decal Firing
PLC6CR - Cone 6 Crystal Glaze Plainsman
PLC6DS - Cone 6 Drop-and-Soak Firing Schedule
QICA - Quartz Inversion Cracking Avoider

"C6MSGL1" Firing Schedule

Mastering Glazes Cone 6

From page 144 in Mastering Glazes.
Step 1 is to provide time for all remaining or residual water in glaze and clay to evaporate. However 220F may not be high enough, 250F is usually needed (and will not fracture ware). This segment should also have a hold, at least 60 minutes.

Step °C °F Hold Time
1 55°C/hr to 105C  99°F/hr to 221F  0 1:58  
2 200°C/hr to 1080C  360°F/hr to 1976F  0 6:51  
3 85°C/hr to 1200C  153°F/hr to 2192F  15min 8:30 Confirm with self supporting cone
4 275°C/hr to 1000C  495°F/hr to 1832F  0 9:14  
5 70°C/hr to 760C  126°F/hr to 1400F  0 12:40  
Start temperature assumed: 25°C or 75°F
"Fahrenheit degrees" is not the same as "degrees Fahrenheit". A 100° reading on a Fahrenheit thermometer is equal to a 37° reading on a Celcius thermometer. But "100 Fahrenheit degrees of temperature change" is equivalent "55 Celsius degrees of change". That is an important distinction to understand the above temperature conversions.

Related Information

Links

Recipes MGBase7 - Raspberry Cone 6 (Mastering Glazes)
From page 102 in Mastering Glazes book
Recipes MGBase2 - High Calcium Semimatte 2 (Mastering Glazes)
Base from Mastering Glazes book page 89
Recipes MGBase1 - High Calcium Semimatte 1 (Mastering Glazes)
From page 86 of Mastering Glazes book
Recipes MGBase3 - General Purpose Glossy Base 1 (Mastering Glazes)
From page 92 in Mastering Glazes book
Recipes MGBase4 - Glossy Base 2 Cone 6 (Mastering Glazes)
From page 96 in Mastering Glazes book
Recipes MGBase5 - Glossy Clear Liner Cone 6 (Mastering Glazes)
From page 97 of Mastering Glazes book
Recipes MGBase6 - Zinc Semimatte Glossy Base Cone 6
From page 98 of Mastering Glazes book
Recipes MGBase8 - Waxwing Brown Cone 6 (Mastering Glazes)
From page 104 in Mastering Glazes book
Recipes MGBase9 - Waterfall Brown Cone 6 (Mastering Glazes)
From page 106 of Mastering Glazes book
Firing Schedules Plainsman Cone 6 Drop-and-hold, Slow Cool
350F/hr to 2100F, 108/hr to 2200, hold 10 minutes, fastdrop to 2100, hold 30 minutes, 150/hr to 1400
Firing Schedules Plainsman Cone 5 Drop-and-Hold Slow-Cool
Oxides Sm2O3 -
Typecodes Oxidation Firing

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy