Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Amblygonite

Formula: (Li,Na)AlPO4(F,OH)

A fluorophosphate mineral.

Related Information

Links

URLs http://en.wikipedia.org/wiki/Amblygonite
Amblygonite at Wikipedia
URLs http://www.handbookofmineralogy.org/pdfs/Amblygonite.pdf
Amblygonite mineralogy data
Materials Amblygonite

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy