Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Magnesite

Formula: MgCO3

A magnesium carbonate mineral. It is quarried in California, Washington, Austria, Russia, Manchuria, Greece and Slovakia and processed from sea water. Sources are reasonably consistent in the CO2 content, but can vary widely in the iron and significantly in the MgO (the analysis given here is theoretical).

Related Information

When both mineralogy and chemistry are shown on a data sheet


This picture has its own page with more detail, click here to see it.

Some material data sheets show both the oxide and mineralogical analyses. Dolomite, for example, is composed of calcium carbonate and magnesium carbonate minerals, these can be separated mechanically. Although this material participates in the glaze melt to source the MgO and CaO (which are oxides), it's mineralogy (the calcium and magnesium carbonates) specifically accounts for the unique way it decomposes and melts.

Links

Materials Camadil 95 Dolomite
Materials KARIBIB Dolomite
Materials Magnesite
URLs http://en.wikipedia.org/wiki/Magnesite
Magnesite at Wikipedia
URLs http://www.handbookofmineralogy.org/pdfs/Magnesite.pdf
Magnesite mineralogy

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy