Description: Unknown

Oxide Analysis Formula Tolerance
CaO 2.40% 0.29
K2O 0.70% 0.05
Na2O 5.90% 0.65
Al2O3 15.50% 1.05
SiO2 74.00% 8.47
LOI 1.50%n/a
Oxide Weight 677.57
Formula Weight 687.89