Yankee Feldspar

Alternate Names: Yankee Spar

Description: Legacy Potash Feldspar

Oxide Analysis Formula Tolerance
K2O 10.21% 0.68
Na2O 3.16% 0.32
Al2O3 17.23% 1.06
SiO2 69.33% 7.24
Fe2O3 0.08% -
Oxide Weight 627.60
Formula Weight 627.60

Notes

Another formula we have is:
K2O 0.61
Na2O 0.35
CaO 0.04
Al2O3 1.06
SiO2 8.43

Related Information

Links

Materials Potash Feldspar
A feldspar having a KNaO content that predominates in potassium.
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.