Alternate Names: WL Rhyolite (Hanks)
Description: From Ron Roy\'s MDT
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 1.16% | 0.16 | |
| MgO | 0.50% | 0.10 | |
| K2O | 4.90% | 0.40 | |
| Na2O | 2.80% | 0.35 | |
| TiO2 | 0.20% | 0.02 | |
| Al2O3 | 11.60% | 0.87 | |
| SiO2 | 76.20% | 9.73 | |
| Fe2O3 | 2.60% | 0.12 | |
| Oxide Weight | 767.37 | ||
| Formula Weight | 767.37 | ||