Whitemud Meta Kaolin

Description: Airfloated sedimentary calcined kaolin

Oxide Analysis Formula Tolerance
SiO2 61.00% 3.04 1
Al2O3 34.00% 1.00 1
Fe2O3 1.65% 0.03
TiO2 0.66% 0.02
CaO 0.20% 0.01
MgO 0.65% 0.05
Na2O 0.13% 0.01
K2O 1.25% 0.04
LOI 0.53%n/a
Oxide Weight 298.62
Formula Weight 300.21

Related Information

Links

Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.