Description: SODIUM BENTONITE GRANULES

Oxide Analysis Formula Tolerance
CaO 1.06% 0.09
K2O 0.36% 0.02
MgO 2.67% 0.33
Na2O 7.08% 0.56
TiO2 0.13% 0.01
Al2O3 16.60% 0.80
SiO2 51.70% 4.23
Fe2O3 3.31% 0.10
LOI 17.10%n/a
Oxide Weight 408.10
Formula Weight 492.27

Notes

Sodium bentonite granules, agglomerated from 325 mesh bentonite. It is fast dispersing and is used as a suspending agent in glazes and a binder for pencil lead.

Specific Gravity: 2.5
pH (5% dispersion): 8.5-10.5
C.E.C. (meq/100g): 82
Dry Brightness (Green Filter): 65
Color: Yellow
% Moisture Content: 12% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 532cps

Related Information

Links

Materials Bentonite
Bentonite can make a clay body instantly plastic, only 2-3% can have a big effect. It also suspends slurries so they don't settle out and slows down drying.
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy