vol356cer

Description: HIGHLY REFINED HECTORITE FLAKE

Oxide Analysis Formula Tolerance
CaO 3.29% 0.08
K2O 0.20% -
Li2O 1.50% 0.07
MgO 23.10% 0.79
Na2O 2.64% 0.06
TiO2 0.20% -
Al2O3 3.05% 0.04
SiO2 52.10% 1.19
Fe2O3 1.13% 0.01
LOI 12.80%n/a
Oxide Weight 119.98
Formula Weight 137.59

Notes

A highly refined hectorite clay supplied as a free flowing flake to ease dispersion. Used as a suspending agent in glazes when high purity and thixotropy are important.

Specific Gravity: 2.5
pH (5% dispersion): 9.5-10.5
C.E.C. (meq/100g): 94
Dry Brightness (Green Filter): 75
Color: White
% Moisture Content: 10% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 8010cps

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy