Description: PURIFIED HECTORITE

Oxide Analysis Formula Tolerance
CaO 3.53% 0.11
K2O 0.40% 0.01
MgO 18.10% 0.76
Na2O 4.65% 0.13
TiO2 0.17% -
Al2O3 3.59% 0.06
SiO2 50.70% 1.43
Fe2O3 0.94% 0.01
LOI 17.80%n/a
Oxide Weight 138.81
Formula Weight 168.87

Notes

An economical blend of beneficiated purified hectorite. Used to promote optimum surface hardening of unfiring ceramic glazes.

Specific Gravity: 2.5
pH (5% dispersion): 9.5-10.5
C.E.C. (meq/100g): 120
Dry Brightness (Green Filter): 75
Color: White
% Moisture Content: 10% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 12,020 cps

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy