Description: FINE GROUND SODIUM HECTORITE

Oxide Analysis Formula Tolerance
CaO 0.65% 0.09
K2O 0.31% 0.03
MgO 2.67% 0.54
Na2O 2.57% 0.34
TiO2 0.16% 0.02
Al2O3 21.08% 1.69
SiO2 63.02% 8.55
Fe2O3 3.25% 0.17
LOI 6.30%n/a
Oxide Weight 764.47
Formula Weight 815.87

Notes

A standard viscosity sodium bentonite with an average particle size ranging between 200 and 325 mesh. It is a general purpose suspending and binding agent, economical for brick and refractory manufacturers.

Specific Gravity: 2.5
pH (5% dispersion): 8.5-10.5
C.E.C. (meq/100g): 92
Dry Brightness (Green Filter): 60
Color: Gray
% Moisture Content: 12% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 170cps

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy