Oxide Analysis Formula Tolerance
SiO2 37.46% 1.06
Fe2O3 0.91% 0.01
Al2O3 59.90% 1.00
TiO2 0.92% 0.02
Na2O 0.20% 0.01
K2O 0.20% -
MgO 0.06% -
CaO 0.05% -
LOI 0.29%n/a
Oxide Weight 169.77
Formula Weight 170.27

Related Information

Links

Materials Mullite
Materials Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc.
Materials Kyanite
Kyanite is a granular material used in the manufacture of ceramics and abrasives. It is notable for low thermal expansion and one-way expansion on heating.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy