Description: CLAY SLURRY
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.10% | 0.01 | |
| K2O | 1.40% | 0.06 | |
| MgO | 0.30% | 0.03 | |
| Na2O | 0.16% | 0.01 | |
| TiO2 | 1.61% | 0.09 | |
| Al2O3 | 24.05% | 1.00 | |
| SiO2 | 60.87% | 4.30 | |
| Fe2O3 | 1.01% | 0.03 | |
| LOI | 10.28% | n/a | |
| Oxide Weight | 379.58 | ||
| Formula Weight | 423.08 | ||
A clean kaolinitic ball clay slurry blend which exhibits superior properties for a variety of uses including fillter applications, ceramic tile body and glaze applications.
Specific Gravity: 1.605
% Solids: 61
Viscosity @ 90F (cps Brookfield, 100 rpm, spindle 3): 200-800
pH @90F: 5.7-6.3
CEC/MBI (meq/100 ml): 8.0-9.0
+200 mesh Residue (%): 0.0-1.0
+325 mesh Residue (%): 0.0-2.0
Soluble Sulfates (ppm): 150-350
Deflocculant Type: Sodium Silicate "N" Brand
Particle Size (% finer than):
5 microns: 86
1 micron: 63
0.5 microns: 53
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |