Description: Pink Stains (MnAl)

Notes

Complete freedom from soluble salts is important to give maximum color dispersion without flocculation of the bodies or slips to which the colors are added.

The colors are produced from calcined mixtures of manganese compounds and alumina. Additions of controlled quantities of other compounds before calcination produce cleaner, brighter shades.

Color Range
-----------
Brown pink through pink to strawberry.

Specific Gravity: 3.5 to 4.0

Stability/Kiln Atmosphere: Exceptionally stable in all types of bodies up to 1450C in both oxidising and reducing conditions.

Compatibility
-------------
Suitable for blending with all types of ceramic colours. Find wide applications in the production of highly stable shades as blends with chrome-antimony-titanium yellows, zircon-vanadium yellows, molybdenum-alumina greys, cobalt-alumina blues and zircon-vanadium blues.

Since these stains tend to be refractory, crawling of overlying glaze can sometimes happen where a 'dry' underglaze lacking sufficient flux prevents the glaze from gaining a foothold on the body underneath.

Cost
----
Relatively low.

Note: This description is taken from information provided by Blythe Matthey and may or may not apply to stains of this family from other companies.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy