Description: STAIN FLUX

Notes

Using stains as underglazes may rob the glaze of its flux causing crawling or dry spots. To alleviate this problem most stain suppliers have underglaze flux compounds to mix with the stain. Typically 10% flux to 90% is used (pinks and browns may require more flux).

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.