1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Spinks Kaolin Low Residue

Description: Western Tennessee Kaolin

Oxide Analysis Formula Tolerance
CaO 0.06% -
K2O 0.04% -
MgO 0.07% -
Na2O 0.02% -
TiO2 2.40% 0.08
Al2O3 38.00% 1.00
SiO2 44.00% 1.97
Fe2O3 0.65% 0.01
LOI 14.00%n/a
Oxide Weight 228.80
Formula Weight 266.05

Notes

Used in ceramics but also adhesives, agricultural, roofing granular, fire-rated applications, refractories and rubber.
Raw color: Light grey.

Related Information

Links

Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

Data

% < 0.5 microns 43%
% Passing 325 Mesh Wet 97.6%
% < 20 microns 97%
% < 10 microns 95%
% < 2 microns 76%
% < 1 micron 62%

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy