Solargil Frit FR4

Description: Low alumina very high alkali frit

Oxide Analysis Formula Tolerance
CaO 7.75% 0.30
K2O 13.01% 0.30
Na2O 11.42% 0.40
Al2O3 1.41% 0.03
SiO2 66.41% 2.40
Oxide Weight 217.18
Formula Weight 217.18

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 122.4 x 10-7 C (Appen)
Frit Softening Point 1000-1300C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy