Description: Turkish Feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 70.20% | 7.00 | |
| TiO2 | 0.25% | 0.02 | |
| Al2O3 | 18.00% | 1.06 | |
| Fe2O3 | 0.11% | - | |
| Na2O | 10.20% | 0.99 | |
| K2O | 0.23% | 0.01 | |
| LOI | 0.30% | n/a | |
| Oxide Weight | 592.90 | ||
| Formula Weight | 594.69 | ||
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |