Silica Yuba

Description: GROUND SILICA FLOUR

Oxide Analysis Formula Tolerance
K2O 0.01% 0.18
Al2O3 0.06% 1.00
SiO2 99.86%
Fe2O3 0.02% 0.21
LOI 0.05%n/a
Oxide Weight 169,915.00
Formula Weight 170,000.00

Notes

Sieve analysis: YubaSil 140# 200# 200F# 300# 325# 325P
------------------------------------------------
Retain on US 60 t
80 t t
100 t t t t t
140 15 5 1 1 t t
200 28 8 4 2 2 t t
270 17 9 4 7 3 1 1
325 23 11 14 8 4 4 2

Bulking Value, gals/lb: .046
Apparent Density (dry uncompacted) 90.6 lbs/cubic foot
pH (37.5% suspension): 6.5
Oil Absorption ASTM D-1483: 20 lbs/100 lbs pigment
Specific Surface Area: 1.05 square meters per gram
G.E. Brightness: 86-88
Specific Gravity: 2.65
Porosity: Non-porous

Related Information

Links

Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy