Silica Volatilized D

Description: SILICA

Oxide Analysis Formula Tolerance
CaO 0.02% -
K2O 0.05% -
MgO 0.02% -
Na2O 0.50% 0.05
TiO2 0.01% -
Al2O3 17.00% 1.00
0.02% -
P2O5 0.05% -
SiO2 82.00% 8.19
Fe2O3 0.10% -
Oxide Weight 598.50
Formula Weight 598.50

Notes

pH: 5-6
Pour Density (kg/m3): 250
Surface Area (m2/g): 15
Particle Size Distribution (D50): 0.5

A low pH, higher Al2O3 variety (Z) is also avalable.

Related Information

Links

Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy