Sericite

Oxide Analysis Formula Tolerance
CaO 0.22% 0.01
MgO 0.31% 0.03
K2O 6.88% 0.25
Na2O 0.10% 0.01
TiO2 0.22% 0.01
Al2O3 29.72% 1.00
SiO2 57.08% 3.26
Fe2O3 0.10% -
LOI 4.65%n/a
Oxide Weight 324.77
Formula Weight 340.61