Selenium

Oxide Analysis Formula Tolerance
Se 100.00% 1.00
Oxide Weight 111.20
Formula Weight 111.20

Notes

A metal of the sulfur group. It is normally added in its pure form to glass batches as a coloring agent for rose or ruby glass or to act as a decolorizer against green iron.

Selenium is also introduced from sodium selenite (Na2O SeO2) or barium selenite (BaO SeO2).

Related Information

Links

Hazards Zirconium Encapsulated Stains Toxicity
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

Data

Hardness (Moh) 4.5
Frit Softening Point 217C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy