Description: A dark buff PCE 27 clay.

Oxide Analysis Formula Tolerance
CaO 0.20% 0.01
MgO 0.50% 0.05
K2O 2.30% 0.10
Na2O 0.10% 0.01
TiO2 1.50% 0.08
Al2O3 25.40% 1.00
SiO2 60.90% 4.07
Fe2O3 1.60% 0.04
LOI 7.50%n/a
Oxide Weight 371.46
Formula Weight 401.57