SA-1 Kaolin

Oxide Analysis Formula Tolerance
CaO 0.06% -
K2O 0.18% 0.01
TiO2 1.50% 0.05
Al2O3 38.40% 1.00
SiO2 45.60% 2.02
Fe2O3 0.40% 0.01
LOI 13.82%n/a
Oxide Weight 228.81
Formula Weight 265.50

Notes

Wilklay SA-1 is a high quality, finely pulverized, airfloat kaolin clay filler with properties specifically selected for the coatings, adhesives, rubber, and other industries. It features low viscosities in aqeous systems and performs as a soft clay in rubber compounds. It is an alternative to Pioneer kaolin.

Specific Gravity: 2.6
Moisture, Max% as produced: 1.0
325 mesh residue, Max: 1.0
GE Brightness, % average: 79.5
pH (28% solids), average: 5.4
Oil Absorption, g/100g clay: 32
Viscosity, 62% solids, cps*, max: 400
Raw Color: Cream

Particle size:
% Finer than 20 microns: 97
10 microns: 91
5 microns: 80
2 microns: 60
1 micron: 47
0.5 microns: 35

Related Information

Links

Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy