Description: Tennessee Ball Clay

Oxide Analysis Formula Tolerance
CaO 0.10% 0.01
K2O 1.60% 0.06
MgO 0.30% 0.03
Na2O 0.10% 0.01
TiO2 1.90% 0.08
Al2O3 29.30% 1.00
SiO2 56.40% 3.27
Fe2O3 0.80% 0.02
LOI 9.50%n/a
C 0.10%n/a
Oxide Weight 315.05
Formula Weight 348.51

Notes

Particle Size (e.s.d.)
125 microns - 0.3
20 microns - 97
2 microns - 65
.5 microns - 35
Modulus of Rupture at 110C
Mn/M2 - 2.2
lbf/in2 - 320
Water Absorption
1120C - 15.0
1220C - 4.0
Shrinkage Dry to Fired
1120C - 8.0
1220C - 12.0
Refractoriness
Cone - 32, 1710C

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.