1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Red Horse Clay

Oxide Analysis Formula Tolerance
CaO 0.45% 0.04
K2O 1.20% 0.06
MgO 0.62% 0.07
Na2O 0.30% 0.02
Al2O3 22.03% 1.00
SiO2 67.59% 5.21
Fe2O3 6.62% 0.19
LOI 1.18%n/a
Oxide Weight 457.50
Formula Weight 462.96

Notes

Another analysis shows 50% SiO2, 28% Al2O3 and 10% LOI, making it appear kaolinitic (thus likely low in plasticity and refractory). It could also be a red fireclay.

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy