R76 Frit

Alternate Names: R76 Alkalifritte

Description: Alkaline Frit

Oxide Analysis Formula Tolerance
K2O 5.43% 0.21
CaO 11.94% 0.79
Al2O3 11.81% 0.43
B2O3 17.60% 0.93
SiO2 53.23% 3.27
Oxide Weight 369.75
Formula Weight 369.75

Notes

Was available in Norway, manufacturer unknown. Info from http://www.potters.org/subject70375.htm

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 1000-1200

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy