1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Putnam Kaolin

Oxide Analysis Formula Tolerance
CaO 0.08% -
K2O 0.20% 0.01
MgO 0.16% 0.01
Na2O 0.24% 0.01
TiO2 0.21% 0.01
Al2O3 37.91% 1.00
SiO2 46.94% 2.10
Fe2O3 0.80% 0.01
LOI 13.47%n/a
Oxide Weight 232.84
Formula Weight 269.09

Related Information

Links

Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

Data

% < 0.5 microns 38%
Firing Shrinkage 18% at cone 9
Water absorption 10% at cone 9

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy