PuraFlow WB Ball Clay

Alternate Names: Black Ball Clay

Description: Light burning clay, very plastic Devon Ball Clay

Oxide Analysis Formula Tolerance
Al2O3 32.00% 1.00
SiO2 47.00% 2.49
K2O 1.00% 0.03
Fe2O3 1.00% 0.02
Na2O 1.10% 0.06
LOI 10.00%n/a
Oxide Weight 261.69
Formula Weight 290.77

Notes

LOI estimated

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.