Premium Feldspar

Alternate Names: Premium Spar

Oxide Analysis Formula Tolerance
K2O 12.12% 0.72
Na2O 3.03% 0.28
Al2O3 18.18% 1.00
SiO2 66.66% 6.25
Oxide Weight 563.22
Formula Weight 563.22

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.